Extruding pellets with more gas hole

yemian5.png

The pellets have more pores, and the rough appearance not only affects the appearance of the feed, but the feed is easily broken into powder during transportation, causing unnecessary waste. It is not easy to sink during the feeding process, and the floating time is long


Reason

Solve solution

Particle swelling coefficient is too large

Adjust moisture, temperature and pressure to reduce the expansion coefficient

Low starch content in the formula

Increase starch content

Super fine thickness

Improve crushing fineness

Excessive moisture in the mold

Reduce the moisture of the material when the mold is released

Mold surface is not smooth

Change the mold